Hastelloy C276 Filler Wire Specification:
| Hastelloy C276 Filler Wire Standard | ASTM B574 / ASME SB574 AMS 5514 |
| Hastelloy Alloy C276 / Wire Dimensions | ANSI/AWCI – 01 -1992 and ASTM E 2016-11 and RRW 360 |
| C276 Hastelloy Wire Length | Cut Lengths: 0.125″ to 72″
No Limit on Spooled Lengths |
| C276 Hastelloy Wire Diameter | 0.0004″ to 0.040″
10 microns to 1.0 mm Other Sizes on Request |
| Wire Density | 8.89 g/cm3 |
| Ultimate Strength (≥ MPa): | 580-750 |
| Wire Resistance (μΩ.m): | as standard |
| Wire Elongation (≥ %): | 28-30 |
| Surface | Polished bright, Smooth, Bare, Enamel, PTFE, Ceramic, Plated |
| Tempers | Tempers range from dead soft annealed to ultra spring temper |
| welded wire mesh | Roll Width: 24inch, 36inch, 1Metre, 48inch, 72inch, or 84inch
Roll Length: 100feet or 150feet |
| wire mesh weaving methods | plain weave, twill weave, dutch weave |
| C276 Wire Technique | Cold Rolled, hot rolled |
| C276 Wire Condition | M, Y, 1/2Hard |
| Offered in a wide range of packages including: | Spool
Reel Coil Bobbin Carrier Custom packaging provided from as low as 1lb to 200lb tapered plastics |
| Wire available in form of | Filler Wire, Flat Wire, Coil Wire, Electrode Wire, Welding Wire, Wire mesh, Knitted wire mesh, filter mesh, mig wire, tig wire, spring wire, stranded and twisted wire |
| Test Certificates | Wire Tensile Testing
C276 Wire Hardness Testing Metallographic Inspection / Investigation Corrosion Testing for Wire Chemical Analysis for 316 Wire Alloy Verification C276 Wire Wrap Testing Wire Elevated Temperature Testing Stress Rupture Testing (Creep) |
Equivalent Grades Hastelloy Alloy C276 Wire:
| STANDARD | WERKSTOFF NR. | UNS | JIS | GOST | EN | OR |
| Hastelloy C276 | 2.4819 | N10276 | NW 0276 | ХН65МВУ | NiMo16Cr15W | ЭП760 |
Chemical Composition of Hastelloy Alloy C276 Wires:
| Grade | C | Mn | Si | S | Co | Ni | Cr | Fe | Mo | P |
| C276 | 0.010 max | 1.00 max | 0.08 max | 0.03 max | 2.50 max | 50.99 min* | 14.50 – 16.50 | 4.00 – 7.00 | 15.00 – 17.00 | 0.04 max |
Mechanical Properties of Hastelloy Alloy B574 C276 Wire:
| Element | Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| Hastelloy C276 | 8.89 g/cm3 | 1370 °C (2500 °F) | Psi – 1,15,000 , MPa – 790 | Psi – 52,000 , MPa – 355 | 40 % |







There are no reviews yet.